Ti, Mn, Fe, Cu, Cr Additive

For Ti, Mn, Fe, Cu, Cr additive, remove package first, then calculate dosage according to the aluminum quantity and alloy yield. Keep molten aluminum temperature at 730-750℃ , put additive into molten aluminum, and shut furnace door for 20-30 minutes, fully mix for 10 minutes by manpower or electromagnet, and slagging-off. Next, adjust temperature and keep in furnace for another 10 minutes, then fully mix again, and refining another 15 minutes with refining flux and slag-off again, finally reach to alloying.

Product Description

Specifications:
Item Model Performance & Application
Titanium Additive 75Ti/80Ti Tablets shaped, it is used for granule refining of aluminum and aluminum alloy, adjust Ti purity in aluminum alloy and improve the tenacity.
Manganese Additive 75Mn/80 Mn/85Mn Tablets shaped, it is used for adjusting Mn content in aluminum alloy to improve alloy strength.
Iron Additive 75Fe/80Fe Tablets sh TTablets shaped, it is used for adjusting Fe content in aluminum alloy.
Copper Additive 75Cu/80Cu Tablets shaped, it is used for adjusting Cu content in aluminum alloy.
Chromium Additive 75Cr/80Cr Tablets shaped, it is used for adjusting Cr content in aluminum alloy.
Aluminum strontium alloy Ai-sr10 Tablets shaped, it is used for lattice variation of aluminum alloy in precision casting.
Guidance:

For Ti, Mn, Fe, Cu, Cr additive, remove package first, then calculate dosage according to the aluminum quantity and alloy yield. Keep molten aluminum temperature at 730-750℃ , put additive into molten aluminum, and shut furnace door for 20-30 minutes, fully mix for 10 minutes by manpower or electromagnet, and slagging-off. Next, adjust temperature and keep in furnace for another 10 minutes, then fully mix again, and refining another 15 minutes with refining flux and slag-off again, finally reach to alloying.

For aluminum strontium alloy, remove package and keep the temperature at 730- 745 after alloying. Keep in stove for 10 minutes, then fully mix and refine for another 10 minutes with high-purity nitrogen or argon gas, finally keep in furnace for 25 minutes and done.

Package and conservation:

2kg/Bag, 40kg/carton, 1000kg/Pallet, keep in ventilated and dry environment. Guarantee period 12 months. Collect packing bag together and dispose them, no burning.